Spanish, level 1 translationSpanish, level 2 translationSpanish, level 3 translationSpanish, level 4 translationSpanish, level 5 translationSpanish, level 6 translationSpanish, level 7 translationSpanish, level 1 stretch translationSpanish, level 2 stretch translationSpanish, level 3 stretch translationSpanish, level 4 stretch translationSpanish, level 5 stretch translationSpanish, level 6 stretch translationSpanish, level 7 stretch translation
Young's Demonstrative Translation of Scientific Secrets · Chapter 266519. To Brown Gun-Barrels
This chapter is not translated yet. You are reading the original.
Rub the barrel, after it is finished, with aquafortis, or spirit of salt diluted in water; leave it by for a week, till a complete coat is formed; then apply a little oil, and after rubbing the surface dry, polish it with a hard brush and a little beeswax.